info@kandbscreeding.co.uk

Drying and flooring

Screed primer: which primer to use before self levelling compound and adhesive

The right screed primer depends on the base. Absorbent sand and cement screed takes a diluted acrylic primer, anhydrite screed takes usually two coats of a primer made for calcium sulphate, and tiles or other non absorbent surfaces take a neat or epoxy primer. PVA is not a substitute. This guide sets out the manufacturers' dilutions, coats and drying times.

Long finished floor screed ready for floor coverings

Many levelling compound failures start before the bag is opened. The base was dusty, the laitance was left on, or the primer was the wrong one, watered down too far, or missing. This guide matches the primer to the base, using UK manufacturers' own data sheets from F. Ball, ARDEX, BAL and Instarmac.

Short answer: prime almost every screed before a levelling compound or cement based adhesive goes on it. Use a diluted acrylic primer on absorbent sand and cement screed and concrete, a calcium sulphate primer on anhydrite screed, usually in two coats, and a neat acrylic or epoxy primer on tiles and other non absorbent surfaces. Do not use PVA. Always follow the data sheet for the exact compound you are laying.

Why screed needs a primer before levelling compound

A screed primer does three jobs. BAL's guide to priming lists them plainly: controlling porosity, preventing chemical reactions between cement based products and gypsum based bases such as anhydrite, and consolidating weak or dusty surfaces.

The porosity job is the one most people underestimate. A dry sand and cement screed acts like a sponge. Pour a levelling compound straight onto it and the screed pulls water out of the mix before the cement can hydrate. F. Ball's data sheet for Stopgap P131 lists preventing "rapid drying" of adhesives and smoothing compounds among its features, and its Stopgap 300 sheet links uncontrolled rapid drying to "surface pin holing, poor flow characteristics, surface imperfections and colour variation". ARDEX describes P 51 as a pore sealer that inhibits air bubbles rising through the compound and extends its flow life.

On dense, smooth surfaces such as glazed tiles or power floated concrete the problem is the reverse: nothing for the compound to grip. There the primer is a bonding bridge.

Some compounds are sold as needing no primer on most bases. ARDEX's ARDITEX NA, for example, lists adhesion to "almost all substrates without priming". Even so, its product page states that "all calcium sulphate-based materials require priming". Check the exceptions on every data sheet.

A primer is not a floor sealer either. Our guide to sealing a concrete floor explains when a bare floor is sealed instead, and why a floor going under new flooring is primed.

Self levelling compound primer by base type

The table uses current UK manufacturers' data sheets. Product names are examples to show what each manufacturer specifies, not the only options. Drying times are at 20°C and run longer in cold rooms.

BaseWhat it needsF. Ball (Stopgap)ARDEX P 51 dilutionDrying before compound
Sand and cement screed, concrete (absorbent)Diluted acrylic to control suctionP131, 1 part to 4 parts water; extra coat on very absorbent bases1 part to 5 parts water for porous or highly absorbent cement screedsP131: 20 to 30 minutes
Power floated concrete, dense screedNeat primer for gripP131 neat, or P141 neat1 part to half a part waterP131 neat: from 60 minutes; P141: from 15 minutes
Anhydrite or other calcium sulphate screedLaitance off, dry to under 75% RH, then two coatsP121: first coat 1 part to 1 part water, second coat neat1 part to 3 parts waterP121: 15 to 30 minutes for coat one, 30 minutes for coat two
Ceramic or quarry tiles, terrazzoNeat acrylic or epoxy bonding primerP141 neat (or P131 neat)Use ARDEX P 82 epoxy primer insteadARDEX P 82: about 4 hours
Plywood overboardingPrimer suited to timberP131, dilutedUndiluted on wood based boardsFollow the sheet for the compound
Old adhesive residuesOnly sound, water resistant residue can stayP141 neat on minimal residues1 part to half a part water; P 82 over residues on bitumen, epoxy or polyurethaneDry fully before pouring

Swipe the table sideways to see every column.

Two practical points sit under every row. The primer has to dry completely before the compound goes on: ARDEX says to leave P 51 until it is "a clear, thin blue film", and F. Ball says primers "must be allowed to dry before applying the smoothing compound". And the base has to be ready: F. Ball's P131 sheet asks for a sound, smooth, dry base below 75% RH with laitance and surface treatments removed.

If you are not sure what the base is, find out before buying anything. A smooth floor poured as a liquid may well be a calcium sulphate flowing screed, and priming it like sand and cement is a mistake to avoid. Our guide to anhydrite screed explains how it differs from cement screed.

Anhydrite screed: primers that stop reactions with cement products

Anhydrite screed is the base where priming matters most. Most levelling compounds and tile adhesives are cement based, and cement products laid directly on a calcium sulphate screed are chemically incompatible with it. BAL's guidance says priming is "crucial" before applying cement based products to anhydrite, to avoid ettringite formation, a reaction between cement and calcium sulphate. The primer forms a film that separates the two.

If you are not sure whether your floor is anhydrite or cement based, our liquid screed brands comparison shows which binder each product uses.

The manufacturers agree on the sequence, if not the exact product:

  1. Let the screed dry. F. Ball's P121 sheet requires calcium sulphate screed to be below 75% RH before priming. Its subfloor preparation guide asks for under 75% RH for textile and resilient coverings and under 65% for wood, or under 0.5% by the carbide method. That carbide limit is much tighter than the 2.5% the same guide allows for cement based subfloors.
  2. Remove the laitance. The weak, chalky skin on the surface must come off by sanding or grinding, and the dust must be vacuumed away. F. Ball's guide warns that laitance is not always fully removed at the first grind and should be checked before any material goes on.
  3. Prime twice. F. Ball specifies two coats of Stopgap P121, the first diluted one to one with water, the second neat once the first is dry. Instarmac's UltraFloor FAQ also calls for two coats of its Prime IT primer on anhydrite. BAL specifies Prime APD at 1:1 for the first coat and neat for the second.
  4. Keep the heating off. F. Ball's P121 and P131 sheets both say underfloor heating must be off for at least 48 hours before, during and after application.

If your floor has underfloor heating in a calcium sulphate screed, get the drying and the laitance removal right first. Our floor preparation service covers grinding, shot blasting and moisture testing to get the surface back to sound, clean screed.

Why PVA is not a substitute

The question "do you PVA a floor before self levelling?" comes up all the time, because PVA is cheap and sits in every builder's van. The manufacturers' answer is no.

BAL puts it directly: PVA "is not recommended for tiling or flooring projects". The reason is moisture. BAL explains that many PVA products re-soften or emulsify when they get wet. A levelling compound brings water onto the floor when it is poured, and BAL says that as cement based adhesives or levellers hydrate they put stress on the softened PVA film, which can severely reduce the bond. BAL "strongly advises" using manufacturer approved acrylic or polymer primers instead.

There is a second reason. None of the levelling compound data sheets we checked lists PVA as an approved primer. Each one names its own primer system, and laying a compound over an unapproved primer means the floor no longer follows the manufacturer's instructions. If the floor fails, that is the first thing anyone will look at.

The same applies to anhydrite. The manufacturers name P121, Prime APD, Prime IT or P 51 at a stated dilution to separate a cement compound from a calcium sulphate screed, and none of them offers PVA as an alternative.

Dilution, coats and drying between coats

Getting the right primer and then mixing it wrong is almost as bad as using the wrong one. These are the habits that keep priming reliable:

  • Measure the dilution. One to four is not one to ten. F. Ball's P131 has three ratios on one bottle: neat for non absorbent surfaces, 1 to 4 for absorbent internal surfaces, and 1 to 7 only for specific external or damp surface systems. Use the one for your base.
  • Brush it in. F. Ball's P131 sheet specifies a paint roller or soft brush, and its Stopgap 300 sheet says not to extend the stated coverage. ARDEX applies P 51 with a soft broom or brush over a clean, dust free surface.
  • Cross the second coat. BAL advises applying a second coat at 90 degrees to the first so nothing is missed.
  • Wait for it to dry. At 20°C, P131 needs 20 to 30 minutes on absorbent bases and about 60 minutes on non absorbent ones. These times stretch in cold weather, and F. Ball and ARDEX both say the surface must be above 5°C.
  • Keep off it. F. Ball warns against excessive foot traffic on a dried primer. Dust walked back onto the film undoes the work.
  • Add a coat where suction is high. P131's sheet says particularly absorbent surfaces may need a further application to reduce pinholes.

Priming and levelling are one job, so plan them together. On our floor levelling work we use the primer the compound manufacturer specifies for the base, then lay the compound once the primer has dried to the stated film. For thin two part compounds over plywood or old tiles, see our latex screed page, and for choosing between a compound and a new screed, our guide to latex vs self levelling compound vs screed.

Before you prime: a quick checklist

  • The screed is dry enough for the compound and the floor covering. Our guide to screeding before flooring covers moisture testing.
  • Laitance, paint, polish, curing agents and water soluble adhesive are removed.
  • Loose or hollow tiles are out and the gaps filled.
  • The base type is known, especially whether it is calcium sulphate.
  • Primer and compound come from the same manufacturer's system.
  • The room is above 5°C and any underfloor heating has been off for at least 48 hours.

Get a fixed price for your floor

If you would rather the priming and levelling were done for you, send us a few photos of the base and tell us the flooring you plan to lay. We will price priming and levelling as one job, so there is no gap between the two trades.

Useful details to include:

  • the floor area in m² and roughly how uneven it is;
  • what the base is, if you know (sand and cement, anhydrite, concrete, tiles or plywood);
  • what is going on top: LVT, vinyl, tiles, carpet or wood;
  • the postcode.

We call back the same day, send a written quote within 24 hours, and agree a fixed price before any work starts. Send your details on our contact page or call 07466 650936.

Sources

FAQs

Frequently asked questions

Can I use the same primer on every floor?

Some primers cover several bases at different dilutions. F. Ball's P131, for example, is used neat on non absorbent surfaces and diluted on absorbent ones. Calcium sulphate screeds often have a dedicated product, such as F. Ball's P121, and ARDEX does not recommend P 51 on asphalt, polyurethane or epoxy coatings, so a single bottle rarely suits every floor. Check the compound's data sheet for the bases it lists.

How long after priming can I pour the levelling compound?

As soon as the primer has dried to a film, and not before. Manufacturer figures at 20°C run from about 15 minutes for F. Ball's P141 to about 4 hours for ARDEX P 82 epoxy primer. In a cold room it takes longer. Do not leave a primed floor for days with people walking on it, because dust and dirt settle on the film.

Do I need to prime before tiling a screed?

Usually, yes. BAL recommends one coat of primer on concrete and sand and cement screeds before tiling to reduce suction, and two coats on anhydrite. Large format tiles also need a flat base, which may mean a levelling compound first. Follow the adhesive manufacturer's primer, since tile adhesive and compound systems are tested together.

What happens if I pour levelling compound without primer?

On an absorbent screed the base draws water out of the mix too quickly. Manufacturers link this to air bubbles, pinholes, poor flow, surface imperfections and colour variation. On anhydrite, BAL warns that cement products react with the unprimed screed, which is why every manufacturer we checked insists on priming it. Taking up a failed compound is far more work than priming would have been.

Can I prime a damp screed?

Not with a standard primer. F. Ball's P121 and P131 sheets both ask for a base below 75% RH. Where a screed cannot dry in time, manufacturers offer surface damp proof membrane systems, such as F. Ball's Stopgap F77, which have their own priming steps. Test the moisture first.

Our services

Services mentioned in this article

Sand and cement screed being laid over underfloor heating pipes

Floor Preparation

Shot blasting, diamond grinding, scarifying and crack and joint repairs. We prepare floor surfaces to the requirements of the client and the finish going on top.

Finished screed floor in a new build room

Floor Levelling

Self levelling compounds and subfloor levelling that turn an uneven screed or slab into a smooth, flat base for LVT, vinyl, tiles and engineered wood.

Large open plan room with a finished floor screed

Latex Screed

Two part latex levelling compound laid a few millimetres thick over overboarded timber, old tiles and uneven concrete, giving vinyl, LVT and carpet a smooth, flat base.

Free, no-obligation quote

Ready to get your floors done properly?